Product Details Supplier Info More products
Download document:

‘Powder coating of perforated plates without holding time’ - .PDF file.

Flat plates, such as perforated plates for control cabinets or top plates, needed a holding time of around 15 minutes at approximately 180ºC. Tests in the in-house Applications Center at Heraeus Noblelight showed that these plates could be heated up in around two minutes, depending on the plate thickness and the coating system.

Click on the link above to download the application note.

 

Application note: powder coating of perforated plates without holding time

Flat plates, such as perforated plates for control cabinets or top plates, needed a holding time of around 15 minutes at approximately 180ºC. Tests in the in-house Applications Center at Heraeus Noblelight showed that these plates could be heated up in around two minutes, depending on the plate thickness and the coating system.

Click on the link above to download the application note.

 

View full profile