The quality of welds depends on the materials used and welding parameters. To help optimizing the welding process, it is necessary to perform very local mechanical characterization of the weld. Nanoindentation and tribology are useful tools for analyzing the effects of the welding process on hardness, elastic-plastic properties and wear resistance.
Download this report to read more.